Root radius and stress concentration

The most common cause of failure is a sharp corner at the root. How large the radius should be, and why larger is not always better.

Sharp cornerR ≥ 0.5 · ttt

The root of the beam carries the highest stress. A sharp corner there raises the stress further and is the single most common cause of failure of snap-fits, above all with rigid, glass-reinforced materials (BASF, Part VI).

Use a fillet radius of at least half the beam thickness, R ≥ 0.5 · t. Beyond that the gain is small, while the thick section can cause voids and sink marks. If sink marks matter, a smaller radius or a radius on the tensile side only is a compromise (BASF, Part VI, Fig. VI-1; Bayer, p. 8, Fig. 9).

Bayer adds a lower limit from internal tests: never less than 0.015 in (0.38 mm) (Bayer, p. 8).

Key points

  • R ≥ 0.5 · t at the root, never below 0.38 mm.
  • Much larger radii cause voids and sink marks.

Open the calculator

Sources

  • BASF Snap-Fit Design Manual, Part VI, p. VI-1, Fig. VI-1
  • Bayer, Snap-Fit Joints for Plastics, p. 8, Fig. 9

Articles summarise the sources in our own words. They do not replace the design guides, your datasheet or tests with real parts.