SnapFitCalc
Open calculator

All articles

Material

Secant modulus and moisture

Why the modulus from the datasheet is often too high for a snap-fit, and why nylon has to be checked twice.

During joining the material is briefly loaded beyond its linear range. The ordinary modulus of elasticity is then replaced by the strain-dependent secant modulus: the stress at the design strain divided by that strain (Bayer, p. 7 and p. 12, Fig. 14). Use the strain on which the undercut was dimensioned.

Nylon takes up moisture. Dry as moulded, the datasheet values apply; at 50 % relative humidity stiffness and holding force drop while the possible deflection increases. Both states should be checked (BASF, Part III).

Key points

  • Forces with the secant modulus at the design strain.
  • Nylon: check dry and conditioned.

Open the calculator

Sources

  • Bayer, Snap-Fit Joints for Plastics, p. 7 and p. 12 (Fig. 14)
  • BASF Snap-Fit Design Manual, Part III, p. III-2

Articles summarise the sources in our own words. They do not replace the design guides, your datasheet or tests with real parts.