Material
Permissible strain and the choice of material
Why the strain at the root decides, where the guide values come from and how to get a value from your datasheet.
The main check of every snap-fit is the strain at the root of the beam while it is deflected by the undercut. It must stay below the permissible strain of the material, otherwise the hook yields or breaks (BASF, Part III; Bayer, Table 1).
Guide values for a single joining operation are listed in BASF Table IV-I and Bayer Table 2. For your own grade, Bayer gives a rule: for one brief joining operation, partly crystalline materials may be strained almost to the yield point, amorphous ones to about 70 % of the yield strain, and glass-fibre reinforced grades without a distinct yield point to about half the elongation at break (Bayer, p. 11, Fig. 13).
If the joint is separated and rejoined often, use about 60 % of these values (Bayer, Table 2). Nylon changes with moisture: check both the dry-as-moulded and the conditioned state (BASF, Part III).
Key points
- The strain at the root decides, not the force.
- Separated often: about 60 % of the one-time value.
- Guide values never replace the datasheet of your grade.
Sources
- BASF Snap-Fit Design Manual, Part III and Table IV-I
- Bayer, Snap-Fit Joints for Plastics, p. 11 (Fig. 13), Table 2 (p. 12)
Articles summarise the sources in our own words. They do not replace the design guides, your datasheet or tests with real parts.